Formosa Plastics Formolene 4142K Extrusion - Sheet - Thermoforming Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Homopolymer with Nucleating, Antistat Additives Applications: Thermoformed cups and container applications. Formolene 4142K DEVELOPMENTAL is a high viscosity homopolymer designed primarily for thermoformed cups and container applications. It contains a unique combination of stabilizers, nucleators and anti-stats that give it an excellent balance of stiffness and impact strength and high clarity. Formolene 4142K offers an advantage in processing over current polypropylenes used for thermoforming, which includes a broader forming window and faster setup time. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Specimens were injection molded according to the conditions specified in ASTM D4101. Information provided by Formosa Plastics Corporation, USA.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|