Formosa Plastics Formolene 5100N Injection Molding Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Homopolymer with ESCR Additives Applications: Various injection molded applications such as closures, small appliances, housewares and toys. Formolene 5100N is a medium viscosity, highly isotactic polypropylene homopolymer designed for various injection molded applications such as closures, small appliances, housewares and toys. It contains a unique combination of stabilizers which give it excellent processability with good stiffness, environmental stress crack resistance, heat performance and minimal odor and taste. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Specimens were injection molded according to the conditions specified in ASTM D4101. Information provided by Formosa Plastics Corporation, USA.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Impact
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|