Formosa Plastics Formolene 6510E Injection Molding Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Impact Copolymer Applications: General purpose injection molding of consumer products, household appliances, lawn and garden items and medical components. Formolene 6510E is a higher impact, medium stiffness copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional stability. It contains a unique blend of stabilizers which give it excellent processing and usage performance. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Specimens were injection molded according to the conditions specified in ASTM D4101. Information provided by Formosa Plastics Corporation, USA.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Impact
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|