Fujipoly Sarcon® Thin-Film TR 45T
Subcategory: Silicone; Thermoplastic
Material Notes: Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of Heat Conductive Silicone Rubber and fiberglass. Information provided by Fujipoly Industries
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dielectric Breakdown
- Dissipation Factor
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flammability, UL94
- Color
- Thermal Impedance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|