Fujipoly Sarcon® Thin-Film GR-TD 25G-Td
Subcategory: Silicone; Thermoplastic
Material Notes: Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
- Volume Resistivity
- Dielectric Strength
- Dielectric Breakdown
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flammability, UL94
- Color
|
|
|
|