Fujipoly Sarcon® Gap Filler Pad GR-n
Subcategory: Silicone; Thermoplastic
Material Notes: Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and make reliable and complete physical contact. GR-Hn has a hardened top surfaceInformation provided by Fujipoly Industries