Aardvark Polymers AARTEL 1000 Rotational Molding Resin
Subcategory: Acetal; Thermoplastic
Material Notes: Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resistance to aggressive chemicals, fuels, and hydrocarbons.Information provided by Gehrig & Associates
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|