Aardvark Polymers AARTEL 850IM Rotational Molding Resin
Subcategory: Acetal; Thermoplastic
Material Notes: Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more freedom in many applications.Information provided by Gehrig & Associates
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|