Aardvark Polymers AARTEL 800 Rotational Molding Resin
Subcategory: Acetal; Thermoplastic
Material Notes: Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of standard colors.Information provided by Gehrig & Associates
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|