Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Subcategory: Acetal; Thermoplastic
Material Notes:
- Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.
- Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled acetals.
- Aardalloy 3300 is a medium viscosity resin with excellent molding characteristics.
- Aardalloy 3300 is available in natural white and may be dry colored to suit.
- Aardalloy 3300 is an excellent choice for fuel tanks, hydraulic reservoirs, brake and fuel system components.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Impact Strength
- Impact
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Izod Impact, Unnotched @ -40°C
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|