SABIC Innovative Plastics NORYL HM3020 PPE + PS (North America)
Subcategory: Polystyrene; Polyphenylene Ether/PPO; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength @ Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Poissons Ratio
- Coefficient of Friction, Static
- Taber Abrasion, mg/1000 Cycles
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- UL File Number, USA
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|