SABIC Innovative Plastics LEXAN 101R Polycarbonate (Europe)
  Subcategory: Polycarbonate; Thermoplastic 
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics. 
Material Notes:  Information provided by GE Plastics for their European product line.  This product is also a part of their North American product line. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Water Absorption
 
- Moisture Absorption at Equilibrium
 
- Water Absorption at Saturation
 
- Linear Mold Shrinkage
 
- Melt Flow
 
- Hardness, Rockwell M
 
- Hardness, H358/30
 
- Tensile Strength, Ultimate
 
- Tensile Strength, Yield
 
- Elongation at Break
 
- Elongation at Yield
 
- Tensile Modulus
 
- Flexural Modulus
 
- Flexural Yield Strength
 
- Izod Impact, Notched
 
- Izod Impact, Notched (ISO)
 
- Izod Impact, Unnotched (ISO)
 
- Izod Impact, Unnotched Low Temp (ISO)
 
- Izod Impact, Notched, Low Temp (ISO)
 
- Charpy Impact Unnotched
 
- Charpy Impact, Unnotched Low Temp
 
- Charpy Impact, Notched
 
- Taber Abrasion, mg/1000 Cycles
 
- Volume Resistivity
 
- Surface Resistivity per Square
 
- Dielectric Constant
 
- Dielectric Strength
 
- Dissipation Factor
 
- Arc Resistance
 
- Comparative Tracking Index
 
- Hot Wire Ignition, HWI
 
- High Amp Arc Ignition, HAI
 
- High Voltage Arc-Tracking Rate, HVTR
 
- CTE, linear 20°C
 
- Thermal Conductivity
 
- Deflection Temperature at 0.46 MPa (66 psi)
 
- Deflection Temperature at 1.8 MPa (264 psi)
 
- Vicat Softening Point
 
- UL RTI, Electrical
 
- UL RTI, Mechanical with Impact
 
- UL RTI, Mechanical without Impact
 
- Flammability, UL94
 
- Oxygen Index
 
- Glow Wire Test
 
- Refractive Index
 
- Haze
 
- Transmission, Visible
 
- Ball Pressure Test, 125 C +/- 2 C
 
- Hot Mandrel Test, 300 C
 
- Water Absorption, 24 hours, mg
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    
    This page displays only the text 
    of a material data sheet.
  
    To see MatWeb's complete data 
    sheet for this material (including 
    material property data, metal 
    compositions, material suppliers, 
    etc), please click the button below.  | 
   
    | 
    
     | 
    
   |   
 |   
  
   |