|   GE Silicones Sanitary 1700™ Construction Sealant  Subcategory: Silicone; Adhesive; Thermoset Close Analogs:  GE Silicones became a part of Momentive Performance Materials in 2006. Material Notes: One-part, mildew-resistant sealant for ceramic tile, showers, tubs, and plumbing fixtures. Cure Method: Acetoxy.  Tack-free time <1 hr.  Peel Strength 20 lb/in.  Sag/slump 0.1 in.
 Data provided by the manufacturer, GE Silicones. 
| | 
    | Available Properties |  
    | Hardness, Shore ATensile Strength, UltimateMaximum Service Temperature, AirMinimum Service Temperature, AirProcessing Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 