GE Silicones IGS3719-D1 Insulating Glass Sealant, Gray
Subcategory: Silicone; Adhesive; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: One-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Cure Method: Alkoxy (Neutral). Tack-free time 0.5 hr. Peel Strength 50 lb/in. Sag/slump 0.1 in. Data provided by the manufacturer, GE Silicones.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Processing Temperature
|
|
|
|