GE Silicones RTV162 White Adhesive Sealant, Non-Corrosive Paste
Subcategory: Silicone; Adhesive; Thermoset
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Key Words: RTV Silicones; R.T.V. Silicones
Material Notes: One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive binding of capacitors, resistors, and integrated circuits to PCBs. Insulate relays, exposed copper wires, terminals. Seal and protect faying surfaces, connectors, and miniature circuits. Data provided by the manufacturer, GE Silicones.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|