GE Silicones IS808 Translucent Adhesive Sealant, General Purpose Paste
Subcategory: Silicone; Adhesive; Thermoset
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Key Words: RTV Silicones; R.T.V. Silicones
Material Notes: One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose, cost-effective sealing and bonding. Cure-in-place electrical insulation. UL approval. Data provided by the manufacturer, GE Silicones.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|