AZDEL Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural applications where high stiffness and impact are desired. Mechanical properties and mold shrinkage measured on flat plaques. Information provided by Azdel.
| Available Properties |
- Specific Gravity
- Filler Content
- Thickness
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Impact
- Impact Test
- Izod Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|