AZDEL Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural, thin wall applications. Commercially available only to European based customers. Information provided by Azdel.
| Available Properties |
- Specific Gravity
- Filler Content
- Thickness
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Impact
- Impact Test
- CTE, linear 20°C
- CTE, linear 100°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Mold Temperature
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|