AZDEL Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: AZDEL® U400-B01N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This material allows highly directionalized reinforcement where loads are in defined planes. Typically it is combined with Azdel chopped and random mat to localized high stress paths, minimizing part weight and cost. For use in semi-structural applications and especially suited to adhesion bonded assemblies. Commercially available only to European based customers. Information provided by Azdel.
| Available Properties |
- Specific Gravity
- Filler Content
- Thickness
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|