GE Silicones N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Key Performance Properties: - Primerless adhesion to many metals and plastics
- Non-corrosive to aluminum and steel per MIL-A-46146A+
- Lower odor cure than conventional silicone sealants
- UL recognition (refer to GE Silicones Tech Info Sheet CDS4320 for additional information)
- One component
- Cures at room temperature
- Excellent electrical insulation properties
- Retains elastomeric properties at temperatures of -60°C(-75°F) to 204°C(500°F) for short periods
- Excellent weatherability, ozone and chemical resistance
Applications: Typical applications include, but are not limited to, sealing vertical joints bonding dissimilar materials such as metal to plastic and glass to aluminum, electrical insulation of wires and terminals, and formed-in-place gasketing.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Tear Strength
- Peel Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Brittleness Temperature
- Dry Time
- Cure Time
- Application rate
- Color
- Consistency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|