GE Silicones RTV133 Black, Flame Retardant, One Component Silicone Sealant
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where resistance to burning of the finished product is a significant design consideration. On exposure to moisture in the air at room temperature, this adhesive sealant cures to a tough, durable, resilient silicone rubber. It utilizes a moisture vapor cure system, which releases an alcohol vapor from the sealant surface during cure. RTV133 sealant offers low odor cure with no unpleasant small or pungent cure by-products. It is, however, somewhat slower curing both in tack-free time and cure-through time than moisture vapor cure silicone adhesive sealants which give off acetic acid vapors as a cur by-product. Because RTV 133 sealant has a paste-like consistency and will flow only with external pressure, it is suitable for use on horizontal, vertical, and overhead surfaces in thicknesses to 6mm (1/4 in.). It has sufficient uncured body to adhere to small objects while cure is taking place. For applications requiring sealant thickness greater than 6mm (1/4 in.), GE Silicones one-component, addition cure or two-component silicone rubber compounds with similar properties are available. Key Performance Properties: - One component product
- Thixotropic paste consistency
- Low flammability - UL94 rating of V-0 or V-1
- Capability to cure at room temperature and ambient humidity conditions
- Self adhesion properties
- Resistance to high temperatures
- Low temperature flexibility
- Excellent weatherability and ozone and chemical resistance
- Excellent electrical insulation properties
- Non-halogen flame retardant
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Brittleness Temperature
- Flammability, UL94
- Dry Time
- Application rate
- Color
- Consistency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|