GE Silicones RTV142 White, Low Volatile, One Component Silicone Sealant
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released from the sealant surface as a by-product of cure. These vapors have low odor and are non-corrosive to metals. An important property of RTV142 is its low volatility. RTV 142 sealant has a thixotropic paste-like consistency. This allows it to be applied to vertical and overhead surfaces without sagging. Since it utilizes a moisture cure system, RTV142 sealant should not be used in thicknesses of greater than 6mm(1/4 in.). When section depths exceed 6mm(1/4in.), GE Silicones one-component, addition cure or two-component silicone rubber compounds are suggested. Mechanical properties for specimen cured 10 days at 25°C and 50% relative humidity. Key Performance Properties: - One component product
- Room temperature cure
- Primerless adhesion to many substrates
- Low odor
- Non-corrosive to metals
- Low volatility
- Low temperature flexibility
- High temperature performance
- Excellent weatherability and ozone and chemical resistance
- Excellent electrical insulation properties
- Non-halogen flame retardant
Applications: The non-corrosiveness to metals and low volatility of RTV142, as well as its paste consistency, make it well suited for critical electronic adhesive, gasketing, and sealing applications where a high level of volatile condensable materials cannot be tolerated.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Collected Volatile Condensable Material
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Tear Strength
- Peel Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Dry Time
- % Total Weight Loss
- Application rate
- Color
- Consistency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|