GE Silicones RTV160 Electronic Grade Silicone Adhesive Sealant, White
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature. These electronic grade silicone adhesive sealants differ somewhat in physical properties including consistency. Key Performance Properties: - Non-corrosive to electronic metals, including copper and brass
- Low odor cure, releasing an alcohol vapor from the sealant surface during cure
- UL recognition
- Retains elastomeric properties for long periods at temperatures from 60°C to 205°C and for short periods up to 260°C
- One-component
- Cure at room temperature
- Excellent electrical insulation properties
- Excellent resistance to moisture, dust, dirt, UV, ozone, and chemicals
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Peel Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Brittleness Temperature
- Dry Time
- Color
- Consistency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|