GE Silicones SS4044P Silicone Primer for use with One and Two Component RTV Silicone Adhesive Sealants, Light Yellow
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants. GE Silicones one-component products offer primerless adhesion to many substrates. Primers are used to help promote adhesion to difficult-to-bond substrates. For most GE Silicones two-component products, a primer is required when an adhesive bond is needed between the silicone rubber compound and a non-silicone surface (see table below). All primers are one-component products requiring no mixing and are supplied ready-to-use as easily pourable solvent solutions. SS4004P and SS4044P primers help promote adhesion to metals (such as aluminum, copper, steel, stainless steel, brass, and galvanized metals), porous materials, unglazed ceramics and wood. SS4004P primer is bright pink, providing easy visual determination of uniform coating. SS4044P primer is virtually identical to SS4004P primer, but is designed for applications where discoloration of the substrate is undesirable. Recommended for 1 and 2 part condensation RTVs. Key Performance Properties: - One-component - no mixing
- Simple handling procedures and equipment for easy use and low processing cost.
- Dry at room temperature and ambient humidity conditions
- Helps promote adhesion to many substrates
- SS4044P, SS4120 and SS4179 primers are transparent to preserve visibility of colorless products.
| Available Properties |
- Specific Gravity
- Solids Content
- Flash Point
- Dry Time
- Color
- D.O.T. Label
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|