GE Silicones SS4155 Silicone Primer for use with One and Two Component RTV Silicone Adhesive Sealants, Blue
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants. GE Silicones one-component products offer primerless adhesion to many substrates. Primers are used to help promote adhesion to difficult-to-bond substrates. For most GE Silicones two-component products, a primer is required when an adhesive bond is needed between the silicone rubber compound and a non-silicone surface (see table below). All primers are one-component products requiring no mixing and are supplied ready-to-use as easily pourable solvent solutions. SS4155 is a general purpose primer for use with any RTV. Key Performance Properties: - One-component - no mixing
- Simple handling procedures and equipment for easy use and low processing cost.
- Dry at room temperature and ambient humidity conditions
- Helps promote adhesion to many substrates
- Blue color of SS4155 primer permits easy visual determination of uniform application
| Available Properties |
- Specific Gravity
- Solids Content
- Flash Point
- Dry Time
- Color
- D.O.T. Label
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|