GE Silicones TSE397 One Component RTV Adhesive Sealant/Coating, Clear/White

 

Subcategory: Silicone; Thermoset; Polymer

Close Analogs:

GE Silicones became a part of Momentive Performance Materials in 2006.

Material Notes:
TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials incorporate a newly developed crosslinking chemistry and are non-corrosive to metallic substrates. They are particularly well suited for electrical/electronic applications.

This series of products differ in consistency, TSE392 is a thixotropic paste, TSE397 is semi-flowable, and TSE399 is flowable. When cured, they retain their elastomeric properties throughout the operating range of temperature from -55C to 200°C (-67F to 392F).

Product Features:

  • Meets the corrosion resistant requirements of MIL-A-46146A
  • Fast cure at ambient temperatures
  • Odor, slight alcohol
  • Outstanding adhesion, including most plastics
  • Outstanding electrical properties
  • Resistant to heat, cold, moisture, UV, ozone and chemicals

Product Benefits:

  • One component, no mixing or de-airing required
  • Soft consistency provides protection against mechanical and thermal shock
  • Excellent electrical insulation
  • Protects against moisture
  • Varying viscosities allow thorough coating around complex assemblies (TSE399) and thicker coatings where required i.e., high voltage components (TSE392 & TSE397).
  • Convenient packaging/dispensing tubes or cartridges.

Available Properties
  • Specific Gravity
  • Viscosity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dry Time
  • Color
  • Consistency
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。