GE Silicones TSE397 One Component RTV Adhesive Sealant/Coating, Clear/White
Subcategory: Silicone; Thermoset; Polymer
Close Analogs: GE Silicones became a part of Momentive Performance Materials in 2006.
Material Notes: TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials incorporate a newly developed crosslinking chemistry and are non-corrosive to metallic substrates. They are particularly well suited for electrical/electronic applications. This series of products differ in consistency, TSE392 is a thixotropic paste, TSE397 is semi-flowable, and TSE399 is flowable. When cured, they retain their elastomeric properties throughout the operating range of temperature from -55C to 200°C (-67F to 392F). Product Features: - Meets the corrosion resistant requirements of MIL-A-46146A
- Fast cure at ambient temperatures
- Odor, slight alcohol
- Outstanding adhesion, including most plastics
- Outstanding electrical properties
- Resistant to heat, cold, moisture, UV, ozone and chemicals
Product Benefits: - One component, no mixing or de-airing required
- Soft consistency provides protection against mechanical and thermal shock
- Excellent electrical insulation
- Protects against moisture
- Varying viscosities allow thorough coating around complex assemblies (TSE399) and thicker coatings where required i.e., high voltage components (TSE392 & TSE397).
- Convenient packaging/dispensing tubes or cartridges.
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Dry Time
- Color
- Consistency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|