Gharda Chemicals GAFONE™ 3500 PES, Unreinforced, Easy Flow
Subcategory: Polyethersulfone; Thermoplastic
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes: Easy flow unreinforced grade for injection molding of thin walled components Characteristics: - Very high rigidity
- Good dielectric properties
- High mechanical strength
- Good dimensional stability
- Good resistance to hydrolysis and sterilization
- Good oxidative stability
- Inherent flame retardance
Applications: - Reusable hypodermic syringes
- Surgical instruments and components
- Printed circuit boards
- Circuit breaker components
- Oil level indicators
- Heat exchanger parts
- Engine components
- Household appliances
- Filter housings
- Sanitary and pipe fittings
Information provided by Gharda.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|