Gharda Chemicals GAFONE™-S 20% Glass Fiber-Reinforced PSU, High Thermal Stability
Subcategory: Polysulfone; Thermoplastic; Polymer
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes: Characteristics: - Good dielectric properties
- High mechanical strength
- Good dimensional stability
- Good oxidative stability
- Inherent flame retardance
- Good hydrolytic stability
Applications: - Printer cartridges
- Mobile phone parts
- Surgical tool trays
- Dental cases
- Business machine parts
- Alkaline battery cell cases
- Household appliances
Information provided by Gharda.
| Available Properties |
- Density
- Filler Content
- Moisture Absorption at Equilibrium
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|