Gharda Chemicals GATONE™-PEEK, 30% Glass Reinforced
Subcategory: Polyketone; Polyetheretherketone (PEEK); Thermoplastic; Polymer
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes: GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements. CHARACTERISTICS: - Outstanding chemical resistance.
- Outstanding wear resistance.
- Outstanding resistance to hydrolysis.
- Excellent mechanical properties.
- Outstanding thermal properties.
- Very good dielectric strength, volume resistivity, tracking resistance.
- Very good radiation resistance.
Information provided by Gharda.
| Available Properties |
- Density
- Filler Content
- Moisture Absorption at Equilibrium
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Volume Resistivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|