Gharda Chemicals Gatone™ 5630CF Polyetheretherketone (PEEK)
Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes:
Characteristics: - Outstanding Chemical Resistance
- Outstanding Wear Resistance
- Outstanding Resistance to Hydrolysis
- Excellent Mechanical Properties
- Outstanding Thermal properties
- Very good Dielectric Strength, Volume Resistivity, Tracking Resistance
- Excellent Radiation Resistance
Applications: - Medical appliances including implantation
- Aerospace application
- Engineering applications like compressor plates, valve seats, moving parts for textile machines
- Electrical and communication cables
- Scientific laboratory instruments
Information provided by Gharda Chemicals
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Hardness, Rockwell M
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|