Gharda Chemicals Gafone™ P4300UF01 Polyphenylenesulfone (PPS)
Subcategory: Polyphenylsulfone; Thermoplastic; Polymer
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes:
Characteristics: - Most Outstanding Impact Resistance
- High Temperature Resistance Tg 222°C
- Continuous use temperature 180°c
- Outstanding Hydrolytic & Chemical Resistance
- Good Clarity
- Flame Resistance
p>Applications: - Medical appliances
- Interior panels of air and surface transportation
- Application involving high impact is required
- Plumbing & hot water pipe fittings
Information provided by Gharda Chemicals
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|