Gharda Chemicals Gafone™ S 1320GF Polysulfone (PS)
Subcategory: Polysulfone; Thermoplastic
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes:
Characteristics: - High Temperature Resistance - Tg 189°C
- Excellent Clarity
- Excellent Mechanical & Electrical properties
- Easy to process
- Very good Hydrolytic Resistance
Applications: - Electrical & Electronic - Head lamp reflectors, Chip tray carriers, battery cases
- Industrial - Milking machine parts, Safety belts
- Medical - Surgical tools, Dialysis membranes
- Membrane applications
Information provided by Gharda Chemicals
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|