GICHEM GIPLENE DX04/V2 Polypropylene - Flame Retardant
Subcategory: Polypropylene; Thermoplastic
Material Notes: PP self-extinguishing, class V2, excellent mechanical properties. Medium injection speed. Information provided by GICHEM Gruppo Industriale Chimico
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Flammability Test
- Oxygen Index
- Glow Wire Test
- Middle Barrel Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|