NEMA G-7 Fiberglass Silicone Laminate Sheet
Subcategory: Silicone; Thermoset; Polymer
Key Words: G7 Fiber Reinforced Composite
Material Notes: This glass-silicone laminate has good electrical properties under humid conditions, excellent heat and arc resistance, and is self-extinguishing. Information provide by Boedeker Plastics.
| Available Properties |
- Density
- Water Absorption
- Hardness, Rockwell M
- Tensile Strength @ Break
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 68°F
- CTE, linear 20°C Transverse to Flow
- Thermal Conductivity
- Maximum Service Temperature, Air
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|