SABIC Innovative Plastics Lexan® 9600 Polycarbonate Sheet
Subcategory: Polycarbonate; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Lexan® 9600 sheet offers improved flammability characteristics than conventional LEXAN polycarbonate sheet. It is formulated to meet the standards of UL Bulletin, Class I. Developed to meet industry flammability codes, LEXAN 9600 sheet is widely used in power tools, electrical appliances, safety equipment and aircraft components. The improved flammability and slightly higher heat deflection temperature of LEXAN 9600 sheet are accompanied by essentially the same physical, electrical, chemical and fabricating properties exhibited by standard LEXAN Sheet. Information provided by Aurora Technologies.
| Available Properties |
- Water Absorption
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 68°F
- Maximum Service Temperature, Air
- Flammability, UL94
- Transmission, Visible
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|