Glastic® Glass-Reinforced Polyester Topsticks
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Glastic Corporation; Glastic LS
Material Notes: Data provided by Glastic Corporation. Pultruded with continuous glass fibers, available in many sizes. Used for motor stators.
| Available Properties |
- Water Absorption
- Flexural Yield Strength
- Shear Strength
- Arc Resistance
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |