Glastic® GLASROD Grade SG-200 Fiberglass-Reinforced Polyester Rod
Subcategory: Polyester, TS; Thermoset; Polymer
Key Words: Glastic Corporation; Glastic LS
Material Notes: Data provided by Glastic Corporation. A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Izod Impact, Notched
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Arc Resistance
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|