Glastic® SG-200 Industrial Lift Magnet
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Material Notes: Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature NEMA GPO-1 products. It is also a superior replacement material for epoxy-bonded mica in layer insulation applications. SG-200 features the following: - Extremely strong
- Excellent retention of properties at elevated temperatures
- Ideal for high temperature applications
- Easily fabricated
- Asbestos-Free
Information provided by Glastic Corporation
| Available Properties |
- Specific Gravity
- Water Absorption
- Tensile Strength @ Yield
- Tensile Modulus
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Notched
- Insulation Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 20°C
- Thermal Conductivity
- UL RTI, Electrical
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
- Electric Strength kV, ASTM D149
- Standard Color
- UL Recognition File Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|