Glastic® 1125 Corrosion-Resistant Panels

 

Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer

Material Notes:
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-free, fiberglass-reinforced polyester resin sheet that offers low smoke generation when exposed to flame. This material has very low water absorption characteristics, along with excellent splash and spill resistance to acids, weak bases and aliphatic hydrocarbons. Grade 1125 is UL classified, has high strength, and has a bright white finish(no painting necessary). Some applications include fume hood liners, chemical storage cabinets and wall surfaces.

Information provided by Glastic Corporation

Available Properties
  • Specific Gravity
  • Water Absorption
  • Tensile Strength @ Yield
  • Tensile Modulus
  • Flexural Strength
  • Compressive Strength
  • Izod Impact, Notched
  • CTE, linear 20°C
  • Thermal Conductivity
  • Flame Spread Index
  • Oxygen Index
  • Smoke Developed
  • Standard Color
  • UL Recognition File Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。