Glastic® 1125 Corrosion-Resistant Panels
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Material Notes: Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-free, fiberglass-reinforced polyester resin sheet that offers low smoke generation when exposed to flame. This material has very low water absorption characteristics, along with excellent splash and spill resistance to acids, weak bases and aliphatic hydrocarbons. Grade 1125 is UL classified, has high strength, and has a bright white finish(no painting necessary). Some applications include fume hood liners, chemical storage cabinets and wall surfaces.Information provided by Glastic Corporation
| Available Properties |
- Specific Gravity
- Water Absorption
- Tensile Strength @ Yield
- Tensile Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Thermal Conductivity
- Flame Spread Index
- Oxygen Index
- Smoke Developed
- Standard Color
- UL Recognition File Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|