Glastic® GoldMember™ Pre-tensioned Fiber Reinforcements
Subcategory: Aramid; Carbon; Glass Fiber
Material Notes: GoldMember™ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and flexibility without adding excessive weight.Information provided by Glastic Corporation
| Available Properties |
- Specific Gravity
- Water Absorption
- Tensile Strength @ Yield
- Tensile Modulus
- Deflection at Failure in.
- Load at Failure, lbs
- Projected Deflection, 200lbs on a 60" span, in.
|
|
|
|