Global S-5000 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Description-good for monofilament Applications-ropes, fishing net, agricultural net and sports net Information provided by Global Polymers Corporation.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Vicat Softening Point
|
|
|
|