Global GG-3245 High Density Polyethylene, Blow Molding Grade
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Description-opacity, medium high stiffness, good impact strength, good chemical resistance Applications- auto parts, bottles, housewares, drums, containers, bottles Information provided by Global Polymers Corporation.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |