Global Atron 601 GF-13 Black Industrial Nylon 6, 13% Glass Filled
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Discontinued Grade
Key Words: Polyamide 6, PA6
Material Notes: Information provided by Global Polymers Corporation.
| Available Properties |
- Density
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|