GLS Corporation Dynaflex® G7736-9 TPE Compound
  Subcategory: Elastomer, TPE; Thermoplastic 
Material Notes:  Bonds to PP General Dynaflex® Information: Dynaflex® TPE Compounds are materials developed to fulfill a broad spectrum of customer specifications. They are designed to provide an economical solution for a wide variety of applications while providing these advantages: - Soft, flexible feel
 - Excellent grip characteristics
 - Good weatherability
 - Easy to process and color
 
 Information provided by GLS Corporation. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Linear Mold Shrinkage
 
- Melt Flow
 
- Hardness, Shore A
 
- Tensile Strength, Ultimate
 
- Elongation at Break
 
- 100% Modulus
 
- 300% Modulus
 
- Tear Strength
 
- Compression Set
 
- Color
 
 
   |   
   |   
 | 
   | 
  
  