GLS Corporation Dynaflex® G7940-1001-00 TPE Compound
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: NSF 51,61 Meets FDA specs Bonds to PP General Dynaflex® Information: Dynaflex® TPE Compounds are materials developed to fulfill a broad spectrum of customer specifications. They are designed to provide an economical solution for a wide variety of applications while providing these advantages: - Soft, flexible feel
- Excellent grip characteristics
- Good weatherability
- Easy to process and color
Information provided by GLS Corporation.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Flammability, UL94
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|