GLS Corporation Versaflex® CL2250 TPE Alloy
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Meets FDA specs Meets USP VI Bonds to PP General Versaflex® Information: Versaflex® TPE alloys create soft touch characteristics that can be customized to create the unique feel that various application require (tactile, slippery, wet grip, silky). Information provided by GLS Corporation.
Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Transmission, Visible
- Color
|
|
|
|