GLS Corporation Versaflex® OM6050X-9 TPE Alloy
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Bonds to Nylon 6 & 6/6 General Versaflex® Information: Versaflex® TPE alloys create soft touch characteristics that can be customized to create the unique feel that various application require (tactile, slippery, wet grip, silky). Information provided by GLS Corporation.