GLS Corporation Versalloy® XL 9070X-1 TPV Elastomer Alloy
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Meets FDA specs Bonds to PP General Versalloy® Information: Versalloy® Elastomer Alloys are designed to deliver high performance in demanding applications. Based on TPV technology, these alloys demonstrate the performance properties of a TPV with improved processability and surface quality compared to standard TPVs. A few of the benefits of Versalloy elastomer alloys: - Excellent surface quality
- Easy processing with excellent flow for long, thin flow paths
- Good compression set
- High tear strength
- Highly colorable
- Low specific gravity
Information provided by GLS Corporation.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|